KN-818C2 Stick Electrode for Low Temperature Resistant Steel
Category: Low Alloy Steel
Specifications
Details
KN-818C2
Type of coating: Iron powder low hydrogen type
It is suitable for welding 540N/mm2 grade steel for low temperature resistance
It is ideal for welding in LNG storage tanks or 3.5% Ni steel for low temperature resistance
Classification
.png)
Application and Features
- It is suitable for welding 540N/mm2 grade steel for low temperature resistance
- It provides high deposition rate, good mechanical properties and X-ray quality welds
- Weld metal contains 3.5%Ni and good impact properties at -75°C
- It is ideal for welding in LNG storage tanks or 3.5% Ni steel for low temperature resistance
.png)
Welding Instruction
- Clean up the contaminations on the steel.
- Dry the electrodes at 350~400°C for 60 minutes before welding.
- Keep arc as short as possible. Take the back step method to prevent porosity at arc start and re-start. (Please refer to Appendix A).
- High heat input will lower the impact value. Please carefully select the welding current.
- The preheat temperature for thick plate is 90~110°C
- It is ideal for welding in LNG storage tanks or 3.5% Ni steel for low temperature resistance
Typical Chemical Composition of Weld Metal (wt%)
.png)
Typical Mechanical Properties of Weld Metal
.png)