Details
KL-916B3
Type of coating: Low hydrogen type
KL-916B3 is suitable for welding Cr-Mo alloy steel
It is ideal for welding high pressure steel pipes and heat exchanger steel pipes, such as ASTM A387Gr.22 and JIS SCMV4
Classification
.png)
Application and Features
- KL-916B3 is suitable for welding Cr-Mo alloy steel
- Weld metal contains 2.25%Cr-1%Mo
- It provides great creep resistance at 550°C
- It is ideal for welding high pressure steel pipes and heat exchanger steel pipes, such as ASTM A387 Gr.22 and JIS SCMV4
.png)
Welding Instruction
- Clean up the contaminations on the steel.
- Dry the electrodes at 350~400°C for 60 minutes before welding.
- Keep arc as short as possible. Take the back step method to prevent porosity at arc start and re-start. (Please refer to Appendix A)
- Preheat and interpass temperature: 160~190°C, PWHT: 675~705°C
- It is ideal for welding high pressure steel pipes and heat exchanger steel pipes
Typical Chemical Composition of Weld Metal (wt%)
.png)
Typical Mechanical Properties of Weld Metal
.png)
Size and Suggested Operation Range (AC/DC±)
View more about KL-916B3 Stick Electrode for Heat Resistant Steel on main site