KS-505 Stick Electrode for Heat Resistant Steel

KS-505 Stick Electrode for Heat Resistant Steel

Category: Low Alloy Steel

Specifications
Details

KS-505
Type of coating: Low hydrogen type
It is ideal for welding high pressure/temperature equipment steel, such as ASTM A219-T9 and A385-P9

Classification


Application and Features 
  • It is suitable for welding Cr-Mo steel
  • Weld metal contains 9%Cr-1%Mo
  • It is ideal for welding high pressure/temperature equipment steel, such as ASTM A219-T9 and A385-P9
Welding Position


Welding Instruction
  1. Clean up the contaminations on the steel.
  2. Dry the electrodes at 350~400°C for 60 minutes before welding.
  3. Keep arc as short as possible. Take the back step method to prevent porosity at arc start and re-start. (Please refer to Appendix A)
  4. Preheat and interpass temperature: 205~260°C,PWHT:725~755°C
Application
- It is ideal for welding high pressure/temperature equipment steel, such as ASTM A219-T9 and A385-P9

Typical Chemical Composition of Weld Metal (wt%)


Typical Mechanical Properties of Weld Metal


Size and Suggested Operation Range (AC or DC±)